Why masterbatch over powder

  • Clean dosing & dust-free: free-foam lines run long continuous shifts; powder metering drifts and creates airborne Sb dust around the feeding zone.
  • Consistent cell structure: pre-dispersed Sb2O3 in a rigid-PVC carrier (K-value 58–65, or EVA/CPE carrier blend) gives uniform nucleating sites → tighter cell-size distribution and smoother skin on Celuka boards.
  • Lot-to-lot stability: each masterbatch lot is QC'd; switching from powder typically lets you cut the kicker (foaming accelerator) dose by 10–15% while holding the same foam density.

Formulation windows

  • Effective Sb2O3 dose: 3–5 phr on the PVC compound (free-foam) / 2.5–4 wt% on the polymer fraction for structural Celuka board.
  • Halogen-antimony synergy: rigid PVC carries chlorine — keep Cl:Sb ≈ 3:1 against the chlorinated paraffin (CP-52/70) or PVC matrix halogen. If a brominated FR is co-added, retune to Br:Sb ≈ 3:1 on effective bromine (not compound weight).
  • Zinc borate (optional): 30–50% of the Sb2O3 loading for smoke suppression where reaction-to-fire class matters (EN 13501-1).

Processing & foaming control

  • ADC + ZnO blowing package: antimony trioxide is mildly nucleating; check foam-gas retention — a fine grade (D50 0.8–1.5 µm) minimises cell-wall rupture vs coarse grades.
  • Pre-dry: after storage >60% RH, dry masterbatch 2–4 h at 70–80 °C to prevent moisture pop (blisters/broken cells).
  • Melt temperature: keep melt ≤190 °C in die/calibrator to limit plate-out and premature gas loss.

QC & acceptance

  • Trial plaques first: verify foam density target (e.g. 0.55–0.65 g/cm³), cell uniformity, skin quality and reaction-to-fire at the final wall thickness (UL94 / EN 13501-1), not a thick lab slab.
  • Per-lot CoA must state: purity ≥99.5%, moisture <0.3%, D50 0.8–1.5 µm, Pb <50 ppm, Fe <100 ppm, whiteness consistency.
  • Documentation: retain 200 g per lot for 12 months; keep lot number ↔ CoA ↔ finished-batch trace for ≥5 years; annual requalification.

供下游 PVC 发泡板/结皮发泡板配方师参考:母粒替代原粉的泡沫控制要点与验收红线。