服务热线:
18971017202
您的位置:首页 >> 新闻中心

Sb2O3 Masterbatch for Flame-Retardant Polycarbonate (PC) Electrical Housings & Distribution Boxes

发布日期:2026-11-21 05:36:17   浏览量:0

Why masterbatch over raw powder

  • Dust-free & metering-accurate: PC dry-blended with raw Sb2O3 powder can segregate and dust during transfer; a PC/SAN-compatible carrier masterbatch holds the active dose and keeps lot-to-lot consistency at 3–5 phr.
  • Anti white-specks on the molded surface: raw powder under-dispersed in translucent/filled PC forms visible specks and grey bloom on glossy housings; fine-grade D50 0.8–1.5 µm in a matched carrier disperses cleanly.

Carrier & compatibility

  • Use a PC or PC/SAN-ABS carrier whose MFI is within ±10–15% of the base PC so flow stays uniform in injection molding; keep viscosity close to avoid a short shot or jetting in thin ribs.
  • Declare the carrier resin and its MFI in the CoA/technical attachment; do not use a polypropylene or low-polarity carrier that phase-separates in PC.

Halogen–antimony synergy (Br:Sb ≈ 3:1 on effective bromine)

  • Pair with brominated flame retardants (e.g. brominated epoxy oligomer / bisphenol-A bis(diphenyl phosphate)-type brominated systems as applicable) calculating the ratio on effective bromine content, not compound weight.
  • Dose ladder 3–5 phr Sb2O3 masterbatch (≈2.5–4 wt% effective Sb2O3 on the polymer fraction); retune Br:Sb to ≈3:1 and confirm with a small moulded plaque before committing a batch.

Moisture control (PC hydrolysis)

  • PC hydrolyses above ~0.02% moisture → silver streaks, loss of impact, viscosity drop. Pre-dry 2–4 h at 80–90°C when storage RH >60%; confirm masterbatch moisture <0.3% in CoA and resin moisture <0.02% at the hopper.
  • Process melt ≤ 270–290°C for PC; avoid over-shearing that raises the melt temperature and triggers degradation.

Process & QC checks

  • Two-roll / plate-out watch: monitor mould fouling and spew between shots; schedule mould cleaning if bloom appears on ribs and live-hinge areas.
  • Screen-pack pressure / screw torque: rising pressure points to filler or carrier incompatibility — stop and re-disperse rather than pushing through.
  • Moulding trial per batch: short-shot ribs, gloss panel, and flash line checked before releasing the lot.

End-product verification (on final wall thickness)

  • UL94 V-0/V-1 on the housing wall thickness (1.5–3.0 mm), not on a thick lab plaque; test knock-down and hot-wire ignition on the finished distribution-box wall.
  • Impact retention ≥85% (Izod/Charpy) vs unfilled reference; -20°C cold drop and 85–105°C heat aging with no surface bloom/plate-out.
  • CTI ≥ 600 V / arc resistance relevant for switchgear & terminal housings; verify dielectric tracking on the finished surface.
  • Confirm heavy-metal migration within limits where the housing is used near food-service or indoor air (screening per CoA).

CoA & retained-sample discipline

  • CoA per lot: Sb2O3 purity ≥99.5%, moisture <0.3%, Pb <50 ppm, Fe <100 ppm, whiteness ΔE <1, D50 0.8–1.5 µm, carrier MFI stated.
  • Retain 200 g per lot for 12 months; keep lot↔CoA↔retained-sample↔moulding-trial traceability ≥5 years with annual requalification and line-trial confirmation.

Supplier note: obtain the masterbatch maker's carrier-MFI and Pb/Fe/whiteness data in writing; treat any undocumented carrier swap as an unapproved change requiring re-qualification.