Antimony trioxide (Sb2O3) acts as the halogen synergist in PVC foam and rigid foam compounds, where the bromine-to-antimony or chlorine-to-antimony ratio is normally held near 3:1 by weight.
Formulation considerations specific to foamed PVC:
- Blowing agent interaction: exothermic blowing agents (e.g. ADC) decompose in the same temperature window where Sb2O3-catalysed dehydrochlorination can start; verify foam cell structure and density across trial runs.
- Cell structure: excessive flame retardant loading can increase melt viscosity and produce coarse, uneven cells; balance loading against expansion ratio.
- Masterbatch route: a masterbatch with a PVC carrier disperses more uniformly into the foam matrix than powder added at the hot mixer, reducing localised burn-through on the skin layer.
- Regulatory: indoor foam profiles may be covered by REACH restriction entries on certain halogenated co-additives; confirm the full package compliance before quoting.
Supplier verification items: Sb2O3 purity (typ. 99.5% min), D50 particle size, whiteness stability, and CoA traceability to the delivered lot. Request test plaques from the same foam formulation before committing to a long-term supply agreement.