Antimony trioxide (Sb2O3) masterbatch is widely specified in halogenated wire and cable compounds, where long extrusion runs make consistent feeding and thermal stability as important as the flame-retardant rating itself.

Feeding and dispersion. Free-flowing masterbatch pellets meter more uniformly than powder in gravimetric feeders, avoiding surges that show up as lot-to-lot LOI variation. Pre-dispersed Sb2O3 in a resin-matched carrier also reduces agglomerates that can initiate carbonized tracking paths in finished cable.

Thermal considerations. Sb2O3 itself is thermally stable at cable extrusion temperatures, but the halogen synergist is not; verify that the masterbatch carrier does not accelerate decomposition. Check VOC/odor data and confirm the supplier's TGA/thermal-degradation profile against your line temperature

** Dielectric QC.** Extrusion moisture below 0.3% per CoA; run volume resistivity and dielectric breakdown on cured/extruded samples, and inspect for surface pitting after damp-heat aging.

Supplier checks. D50/D97 particle size distribution, Sb2O3 assay >= 99.5%, whiteness consistency for sheath compounding, halogen-free certification if requested, and batch traceability via CoA. Run a continuous extrusion trial at target loading before approving volume supply.