PC/ABS blends are widely used for device housings, dashboard trim and power-tool bodies. Antimony trioxide (Sb2O3) masterbatch can be compounded with brominated FRs (typically decabromodiphenyl ether or tetrabromobisphenol-A oligomers) in the ABS phase and at the blend interface, but the alloy has its own constraints that pure ABS does not.
Key formulation points: - Br/Sb molar ratio: keep the classic ~3:1 window; blends with high PC content often need 5–7 wt% brominated FR plus 2–3 wt% Sb2O3 to reach UL94 V-0 at 1.6 mm. - PC is hydrolysis-sensitive. Sb2O3 should be low-moisture (CoA moisture < 0.3%) and pre-dried pellets dried 80–100 °C / 2–4 h before molding, otherwise molecular weight drops and impact strength falls. - Dispersion: the masterbatch carrier (usually SAN or ABS) must match the blend's MFI so the FR stays in the ABS phase; poor matching pushes Sb2O3 into the PC phase and causes haze. - Heat stability: compounding at 240–260 °C is close to deca-BDE limits; check TGA data and use low-volatility grades for thin-wall parts.
Incoming QC checks against the CoA: 1. Sb2O3 assay (≥ 99.5% for flame-retardant grades). 2. Particle size D50 0.8–1.5 µm, D97 ≤ 5 µm — coarse particles raise plate-out and lower impact. 3. Whiteness consistency between lots, since tinted housings amplify shade drift. 4. Moisture and volatile content < 0.3%.
Line trial: verify notched impact retention (blend FR systems can cost 15–30% of impact), check for die build-up after 30–60 min running, and confirm gloss on textured surfaces. Keep retained samples per lot for one year so regrind or warranty questions can be traced back to a CoA.