Rigid PVC window and door profiles are extruded with lead-free (Ca-Zn or tin) stabilizer systems, and antimony trioxide is only introduced when the profile spec demands a higher fire rating. A pre-dispersed Sb2O3 masterbatch in a PVC-compatible carrier avoids dust handling and keeps filler dispersion uniform on the line.

Formulation and dosing points

  • Carrier match: pick a masterbatch carrier with the same K-value family as the rigid PVC blend so the hot-mix and extrusion rheology do not drift when Sb2O3 is introduced.
  • Stabilizer pairing: Sb2O3 does not replace a heat stabilizer; when paired with Ca-Zn systems, confirm the pigment/paste supplier has tested any interaction (zinc antimonate formation can whiten the surface over time).
  • Plate-out watch: any added fine filler accelerates die plate-out; check the calibration table and die Lips cleaning interval after a trial run.
  • Dose: follow the halogen source ratio (≈3:1 halogen:Sb atomic) and verify the final profile class against the relevant fire standard (e.g., DIN 4102 B1 where specified).

Weathering and color

  • Window profiles are UV-critical. Run co-extruded cap-stock samples through QUV or xenon arc exposure before committing: confirm that ΔE color drift stays within the agreed tolerance with the Sb2O3 loading in the substrate.
  • Fine-particle grades (D50 ≈ 0.8–1.5 µm) cut the loading needed for the same fire class and minimize impact-strength loss.

Supplier qualification checklist

  • CoA per lot: purity ≥ 99.5 %, moisture < 0.3 %, and particle size D50/D97 in range.
  • Impact retest on extruded profiles at every dose change; keep one-year retained samples of each production lot for after-sales traceability.