服务热线
18971017202
Masterbatch route for PET strapping tape and PA6 industrial yarn, where the polymer is drawn to high tenacity and any inorganic coarse particle becomes a break point on the draw line.
Carrier and dosing - PET tape grades: use a low-moisture PET carrier masterbatch matched to the tape IV (intrinsic viscosity) range; PA6 technical yarns: use PA6 carrier with a matched relative viscosity. Generic EVA/PP carriers cause interface haze and draw-line breaks. - Dose 3.5–5 wt% Sb2O3 on polymer fraction with Br:Sb ≈ 3:1 molar against the brominated co-agent; retune after any resin or co-agent change. - Fine grade only: D50 0.8–1.5 µm. Coarse tails (D97 > 45 µm) show up immediately as filament breaks and strap splitting at draw ratios above 4x.
Processing gates - Pre-dry PET base resin to <0.005% moisture and the masterbatch-added blend to spec before spinning/extrusion; PET hydrolyzes fast at 280–300 °C and IV drop is permanent. - PA6 needs controlled moisture (2–3.5%) upstream but dry masterbatch feed; watch screw compression for dispersion uniformity, ash uniformity ±10% across the web/tape. - Spinnerette and draw-roller plate-out watch: fine-grade only, surface-treated grades recommended for draw ratios >4x.
Qualification (CoA) - Purity ≥99.5%, D50 0.8–1.5 µm, moisture <0.3%, Pb <50 ppm, Fe <100 ppm, whiteness consistency for tinted straps. - Per-lot retained samples (200 g, 12 months); annual requalification if grades or carriers change.
Trial QC - Single-end tenacity and elongation at break on yarn; strap tensile and peel on tape; burn (LOI/UL94 HV) on the finished article only, not on undrawn feedstock.