Application Context

PVC corrugated conduit and spiral-wound looms protect automotive and industrial wiring harnesses. They must hold a rated reaction-to-fire class while surviving engine-bay heat, abrasion, and vibration without brittle cracks or surface bloom.

Masterbatch vs Powder

  • Why masterbatch: dust-free dosing on fast extrusion lines, consistent lot-to-lot antimony loading, better dispersion in the thin-wall corrugation profile, and fewer white specks at the corrugation ribs where stress concentrates.
  • Carrier match: rigid PVC carrier matched by K-value (56–65) or a CPE/EVA polarity-matched carrier so the let-down resin stays compatible without separate dry-blending.

Dose & Synergy

  • Dose 3–5 phr Sb2O3 on the PVC compound.
  • With chlorinated paraffin CP-52/70 halogen source, keep Cl:Sb ≈ 3:1; retune to Br:Sb ≈ 3:1 if a brominated flame retardant is substituted.
  • Add zinc borate 3–8 phr when smoke suppression (e.g. ISO 6722 / UL interior) is a requirement; re-tune the halogen–antimony ratio downward 5–10%.

Processing Checks

  • Melt ≤ 190°C to limit plate-out and PVC degradation.
  • Pre-dry masterbatch 2–4 h at 80°C after storage above 60% RH.
  • Watch die and corrugation calibrator plate-out; run a 2-hour line trial before batch commit.
  • Verify dispersion with a two-roll mill bench check and filter-pressure/ash-uniformity (±10%) screening.

Qualification & CoA

  • CoA per lot: purity ≥ 99.5%, moisture < 0.3%, Pb < 50 ppm, Fe < 100 ppm, D50 0.8–1.5 µm, whiteness consistency.
  • Final-part re-tests: reaction-to-fire at rated wall thickness, cold-bend (ISO 6722), dielectric strength, abrasion, and heat aging (70°C/28 d) with no bloom or brittle failure.
  • Retain 200 g per-lot sample for 12 months for traceability.

Takeaway

Masterbatch route for PVC harness conduit improves dosing consistency and surface quality; qualification hinges on melt-temperature control, halogen–antimony ratio retuning, and per-lot CoA plus final-part fire and cold-bend re-testing.