Application Context

High-plasticizer flexible PVC (DINP/DOA/ESO at 40–60 phr) used for inflatable products, pool liners, and coated tarps. These parts see sustained outdoor UV, low-temperature flexing, and seam-weld integrity — so flame retardancy must be balanced against blooming, plasticizer migration, and weld-line strength.

Dosing & Formulation

  • Masterbatch over powder is preferred: dust-free loading on high-plasticizer lines, better lot-to-lot antimony content consistency, and fewer white specks in thin 0.2–0.5 mm skins.
  • Carrier: flexible-PVC/EVA type with declared plasticizer content; match carrier softness to the base resin so melt flow stays uniform.
  • Dose window: 3–5 wt% Sb2O3 on the polymer fraction; retune the halogen ratio to Cl:Sb ≈ 3:1 when the halogen source is chlorinated paraffin CP-52/70 (flexible PVC usually avoids brominated FRs for cost and bloom).
  • For thin translucent liners, cap effective Sb2O3 toward the low end and use fine grade D50 0.8–1.5 µm to limit haze.

Processing & QC Watch-Points

  • Pre-dry masterbatch 2–4 h at 70–80 °C after storage above 60% RH — moisture in flexible PVC causes splay and weld-line voids.
  • Keep melt ≤190 °C; watch die/calender plate-out and white bloom on cooled surfaces.
  • Weld/seam check: high-frequency or hot-air weld-line strength must not drop >10% from masterbatch addition — verify on trial skins.
  • Low-temperature: cold-flex / brittleness test at −20 °C on final film.
  • Weathering: QUV/xenon ΔE and tensile retention after 500 h — antimony oxide can catalyse UV degradation if overloaded.
  • Migration: plasticizer bloom test 22 h/70 °C; ensure Sb2O3 fine grade does not aggravate surface exudation.

CoA Verification (per lot)

  • Sb2O3 purity ≥99.5%, moisture <0.3%, Pb <50 ppm, Fe <100 ppm.
  • D50 0.8–1.5 µm, D97 upper bound, whiteness consistency.
  • 200 g retained sample per lot, 12 months.
  • Reaction-to-fire (UL94 / EN 13501-1) on finished skin thickness, not on raw compound.

Supplier Checklist

Ask for: two-roll dispersion test, per-lot trial-skin haze/gloss data, weld-strength and cold-flex results, and a statement of carrier plasticizer type/level. Reject any grade whose D50 exceeds 1.5 µm for thin-skin applications.