Application: Encapsulant layers in solar modules — where optical clarity, PID-resistance and fire retardancy must coexist.
Why Masterbatch Over Powder
- Dust & contamination control: Powder Sb2O3 risks light-scattering inclusions that raise haze and lower module efficiency.
- Lot-consistent dosing: Masterbatch delivers reproducible 2.5–4 wt% effective Sb2O3 per batch, tightening EVA/POE encapsulation performance.
- Dispersion: Twin-screw compounding ensures sub-visible particle spread, avoiding pinhole/void defects that trigger cell micro-cracks.
Formulation Pointers
- Carrier: EVA (VA 28–33%) or POE carrier matched within ±10–15% MFI of the base encapsulant to prevent melt-flow mismatch.
- Ratio: Br:Sb ≈ 3:1 (on effective bromine) with a brominated co-additive; re-tune when switching halogen source.
- Fine grade: D50 0.8–1.5 µm — coarser grades raise haze and risk cell-encapsulant interface voids.
Processing / QC Checks
- Pre-dry 2–4 h at 70–80 °C when storage RH >60% — moisture hydrolyses EVA and promotes bubbles.
- Melt ≤ 180 °C during film extrusion; watch die/roll plate-out.
- Haze < 2–3% on trial film before committing a batch.
- Gel content & crosslink density per lot (peroxide cure window).
- Module-level: PID resistance (85 °C / 85% RH), UV/ΔE weathering, peel adhesion after 1000 h damp-heat.
CoA Verification
Purity ≥99.5% · Moisture <0.3% · D50 0.8–1.5 µm · Pb <50 ppm · Fe <100 ppm · Whiteness ΔE <1.
Retain 200 g per lot for 12 months; annual re-qualification. Qualify each new lot with a mini module trial before production commitment.
Supplier qualification checklist: batch traceability, per-lot CoA, retained-sample programme, line-trial evidence.