Sb2O3 Masterbatch for Flame-Retardant Acrylic (PMMA) & Extruded Optical Sheets

发布日期:2026-11-21 05:35:46   浏览量:0

Masterbatch over powder — why

Cast and extruded PMMA sheets (2–6 mm, signage, diffusers, UV-stable panels) demand optical clarity and a clean, dust-free surface. Loose Sb2O3 powder causes haze, agglomerates, and white specks on the sheet face. A matched PMMA-carrier masterbatch delivers fine dispersion, consistent per-lot dosing, and a smooth surface — the recommended route for optical-grade fire-rated sheets.

Carrier selection

  • Use a low-MFI PMMA (cast-grade / extrusion-grade acrylic) carrier matched to the sheet resin's flow; mismatched carrier creates melt streaks and warpage.
  • For co-extruded cap layers, keep the masterbatch only in the core or the cap depending on where fire rating is required — never dose it into both and double-count.

Dose & halogen–antimony synergy

  • Effective Sb2O3 loading: 3–5 wt% on the polymer fraction; thin sheets (≤2 mm) need the top of the window to reach the target reaction-to-fire class.
  • Maintain Br:Sb ≈ 3:1 by mole on effective bromine (from the brominated synergist actually present), not on compound weight.
  • Optional zinc borate at 30–50% of the Sb2O3 level to cut smoke and reduce afterglow on cast sheets.

Processing & quality checks

  • Pre-dry the masterbatch 2–4 h at 70–80 °C if stored above 60% RH; acrylic is moisture-sensitive and wet feed causes splay marks.
  • Keep melt ≤ 260 °C; watch die/roller plate-out and surface bloom on cooling.
  • Trial-plaque checks before batch commit: haze < 2–3%, light transmittance ≥ 88%, no white specks, ΔE < 1 vs control.

CoA verification (per lot)

  • Sb2O3 purity ≥ 99.5%; moisture < 0.3%; fine D50 0.8–1.5 µm (anti haze); Pb < 50 ppm; Fe < 100 ppm; whiteness ΔE < 1.
  • End-product verification on the finished sheet, not the pellet: reaction-to-fire class at the target wall thickness, vertical burn, and UV/QUV retention.
  • Keep a 200 g per-lot retained sample for 12 months; requalify annually or on resin/source change.