PC electrical enclosures, junction boxes and smart-meter housings demand UL94 V-0/5VA at thick walls — but Sb2O3 chemistry is constrained on PC: the carbonate backbone hydrolyzes in the presence of acidic residues, and halogen/Sb synergies must be chosen carefully.

Constraints & formulation - Antimony-halogen on pure PC risks hydrolysis-driven embrittlement and haze; industry practice favors brominated PC oligomers or aromatic bromides designed for polycarbonates, with Sb2O3 only where melt chemistry is verified tolerant. - Typical working zone: effective Sb2O3 2–4 wt% on polymer fraction, Br:Sb ≈ 3:1 calculated on effective bromine; verify retention of notched impact within −10% and MFI drift within −10–15% before line commit. - Pre-dry PC at 110–130°C to moisture <0.02% — antimony co-additives accelerate hydrolysis when moisture is uncontrolled. - Melt temperature ≤300°C; brominated systems decomposing above ~330°C cause plate-out and corrosion.

QC & supplier checks - Trial plaques: UL94 V-0/5VA at final wall thickness, not pellets; haze (ΔY) and impact on aged samples (70°C/168h). - CoA: purity ≥99.5%, moisture <0.3%, D50 0.8–1.5 µm, Pb <50 ppm, Fe <100 ppm; chloride residue specification especially relevant to PC. - 200 g per-lot retained sample, 12 months; annual requalification with impact retention report.

在线咨询 联系方式 二维码

服务热线

18971017202

扫一扫,关注我们