Antimony trioxide (Sb2O3) is used in rigid PVC window profiles as the halogen-synergy component of the flame-retardant package, almost always together with a brominated or chlorinated co-additive. Sb2O3 alone adds little flame-retardant effect; the ratio and dispersion quality decide the result.
Dosage and synergy
- With brominated co-additives, keep the Sb:Br mass ratio near 1:3; against chlorine donors the classic window is 1:3 to 1:4. Outside this window, more Sb2O3 only raises cost and impact loss.
- Typical totals in profile compounds: 3-6 phr combined FR package, tuned against the EN 13501 or UL 94 V-0/V-1 target at the profile's wall thickness.
Stabilizer interaction
- Modern profiles run Ca/Zn or OBPb-free stabilizers. Sb2O3 is chemically inert toward calcium/zinc soap stabilizers, but acidic impurities (As, Pb traces out of spec) accelerate zinc burning and early yellowing; require assay >= 99.5% with As/Pb trace limits on the CoA.
- Sb2O3 does not replace lead stabilizer functions; do not treat it as a stabilizer substitute in lead-free conversions.
Dispersion and impact loss
- Rigid PVC is notch-sensitive: undispersed Sb2O3 agglomerates act as impact modifiers' counterweight. Prefer a masterbatch at 60-80% active in a PVC/K-S value-matched carrier, pre-dispersed to <5 um domains.
- Check the Charpy/IZOD impact retention after compounding; a drop beyond the agreed tolerance (typically >10%) usually signals poor dispersion or overloading, not the Sb2O3 grade itself.
Procurement checkpoints for profile extruders
- Whiteness >= 95 and consistent D50 particle size from lot to lot (visible color drift in light-colored profiles starts here).
- CoA per lot with assay, As/Pb traces and laser particle-size distribution.
- Sealed retained samples 12-24 months for dispute arbitration.
- Supply reliability: dual-supplier qualification before committing long-run profile programs.