Sb2O3 masterbatch for rigid PVC window profiles.

发布日期:2026-11-21 05:34:37   浏览量:0

Heat stability: two-roll mill / torque rheometer test; torque drop of 10-15% versus blank PVC marks the performance red line. Zinc-calcium stabilizer pairing is standard; check plate-out risk — excessive Sb2O3 or poor surface treatment deposits on rolls and dies.

Weathering: require QUV or xenon-arc test data (chalking, ΔE<3 after specified hours). Granulometry D50/D97, Sb assay ≥99.5%, moisture <0.3% on CoA. Trial extrusion: gloss uniformity and impact strength ((Charpy), no silver streaks. Supplier qualification includes one-year retained samples.

All loads verified by duplicate CoA review and incoming inspection each batch.