服务热线:
18971017202
您的位置:首页 >> 新闻中心

Sb2O3 masterbatch for silicone rubber compounds: peroxide-cure interference, acid-treated vs. standard grades, dispersion QC and CoA qualification notes

发布日期:2026-11-21 05:34:46   浏览量:0

Application note for rubber compounders using antimony trioxide (Sb2O3) masterbatch in HTV/LSR silicone rubber compounds requiring flame retardancy (UL 94 / cable specifications).

Peroxide-cure interference. Antimony trioxide surfaces can interfere with peroxide curing systems (e.g., 2,4-dichlorobenzoyl peroxide for HTV): acidic surface groups on some grades retard cure, raising scorch time and lowering crosslink density. Prefer acid-washed or surface-treated fine grades, and re-tune the peroxide dosage with a lab scorch/cure curve (moving-die rheometer ODR/MDR) whenever a new Sb2O3 grade or lot enters the recipe.

Grade selection for silicones. Standard grades can carry trace metals (Fe/Pb) that discolor translucent silicone and add ionic contamination; for medical- or food-adjacent grades specify low-Fe, low-Pb assays. Fine-particle grades (D50 roughly 0.8-1.0 micron) disperse more easily in fast mixer cycles but are more prone to blooming; choose the grade together with the dispersion equipment and post-cure regime.

Dispersion and processing. Add the masterbatch early in the mixing cycle so the filler is wetted before structuring oils or fuming silica; avoid exceeding the mixer chamber temperature that would prematurely activate the peroxide. Check dispersion with a torn-surface or thin-sheet light test: streaks or white specks indicate undispersed masterbatch, which shows up downstream as inconsistent flame performance and die build-up in extrusion.

Flame-retardant package. Silicone's inherent fire performance improves markedly once halogen-free mineral synergists (zinc borate, platinum cure systems) are combined with small Sb2O3 doses; confirm the combined package against UL 94 V-0 and the specified smoke density limits, then keep the ratio fixed in QC documents because small drifts in the Sb2O3 share move the LOI and smoke results measurably.

Supplier qualification. CoA items to verify per lot: Sb2O3 assay, moisture (<0.3%), particle-size distribution (D50/D97), surface-treatment type if any, and whiteness for light-colored compounds; retained samples 12-24 months; re-run an MDR cure check per new lot before releasing the batch to production.

在线咨询 联系方式 二维码

服务热线

18971017202

扫一扫,关注我们