服务热线
18971017202
Antimony trioxide (Sb2O3) is the standard synergist with brominated flame retardants in polyethylene terephthalate (PET) applications, including electrical housings, connectors and automotive interior parts. Masterbatch delivery in a PET or PBT carrier simplifies metering but introduces specific risks.
Hydrolysis of PET. PET is moisture-sensitive; residual water above about 0.02% causes chain hydrolysis and molecular-weight loss during melt processing. Both the resin and the antimony masterbatch must be pre-dried (typically 120–140 °C for 4–6 h for PET). Masterbatch pellets must be supplied with moisture certification, as carrier-bound moisture is a frequent cause of embrittlement.
Dosage ratio. With aromatic brominated retardants such as brominated epoxy oligomers or decabromodiphenyl ethane, a molar Br:Sb ratio of approximately 3:1 is standard. Glass-fibre-reinforced grades require dose calculation on the polymer fraction, not final compound weight.
Catalytic residue interaction. Sb2O3 residues can interact with residual antimony acetate catalyst and antimony-based condensation catalysts already present in PET, slightly shifting color (grey tinge) and crystallization rate. Formulators should run colorimetry (ΔE) and crystallization half-time checks.
Supplier qualification (CoA). Required checks per lot: antimony content ≥99.5%, D50 0.8–1.5 µm (fine grades for thin walls), moisture <0.3%, lead <50 ppm and iron <100 ppm, carrier MFI matching the PET grade being processed.
Line quality control. Conduct dispersion checks on molded or spun specimens, monitor for filter/screen blockage in thin-wall molding, and retain a sample of every lot for traceability.
Why is pre-drying critical for antimony masterbatch in PET? Residual moisture hydrolyzes PET during processing; drying both the resin and masterbatch prevents embrittlement and IV loss.
How is Sb2O3 dose calculated in glass-filled PET? The ~3:1 Br:Sb molar ratio is applied to the polymer fraction, then total loading is adjusted for fibre content.