Automotive interior components — instrument panels, door trim, center consoles, and pillar covers — must meet OEM flammability specifications (most commonly FMVSS 302) while retaining dimensional stability and low VOC emissions across a wide service temperature range.
Formulation in TPO, PVC and polyurethane interior substrates
- In TPO interior skins and substrates, a polypropylene-based Sb2O3 masterbatch matches the host resin MFI and disperses cleanly without blooming onto soft-touch coatings.
- Select fine particle grades (D50 0.8–1.5 µm) to minimize haze on grained surfaces and to avoid white speck defects under cabin lighting.
- Combine with brominated or chlorinated co-additives at roughly a 3:1 halogen-to-antimony molar ratio; for interior PVC grades the chlorine inherent in the polymer lowers the additional halogen co-additive requirement.
Heat aging, fogging and color stability
- Sun-exposed zones reach sustained 85–105°C surface temperatures; run 500–1,000 h heat-aging to confirm the masterbatch carrier does not volatilize or contribute to windshield fogging.
- Check color fastness of light-gray and beige formulations by comparing ΔE before and after aging against a retained standard plaque.
Supplier and CoA verification for Tier 1 molders
- CoA: purity ≥99.5%, moisture <0.3%, Pb <50 ppm, Fe <100 ppm.
- D50/D97 size distribution consistent within ±10% between lots.
- For light interior shades request whiteness ≥96 and per-lot retained samples (200 g, 12 months).
- Confirm a two-roll bench dispersion check precedes each molding trial, plus a QUV weathering comparison against a retained plaque.
A qualified automotive interior grade is defined by reproducible dispersion, controlled VOC/fogging behavior, and a fully traceable batch record rather than by flame-retardant loading alone.