Polypropylene corrugated sheet (plastic cardboard) and twin-wall sunlight board are thin-walled extrusions (0.2–0.5 mm per wall), so the flame-retardant package has to reach V-2 or better without killing flex stiffness across the flute lines.
Dosing. With a halogen co-additive, hold the Br:Sb molar ratio near 3:1 on the polymer fraction. Typical Sb2O3 dose is 3–5% via masterbatch. Because the sheet surface is visible on both faces, fine-grade antimony trioxide — D50 about 0.8–1.5 µm — keeps the surface free of white specks and color drift, which powder addition at these thicknesses tends to produce.
Carrier. Match the carrier PP melt index to the sheet resin (MFI 8–20 for typical corrugated grades). A mismatch shows up as plate-out at the die lip and gels in the skin, which on twin-wall board concentrates at the knuckle points.
Processing checks. Pre-dry masterbatch after storage above 60% RH (80–100 °C, 2–4 h). Watch the breaker-plate pressure: a rising trend is the usual first sign of poor dispersion. Keep the extruder below the decompositions limits of the brominated co-additive (DBDPE, for example, is tolerant to about 325 °C).
Qualification. Per-lot CoA: purity ≥99.5%, D50 0.8–1.5 µm, moisture <0.3%, Pb and Fe limits as specified. Run the flexural modulus and an LOI/UL94 strip on finished sheet, not pellets, and keep a 200 g retained sample per lot for 12 months.