Technical application note for film and thermoforming converters
1. Why masterbatch over powder in transparent film
- Dispersion & haze control — powdered Sb2O3 agglomerates cause white specks, gel and haze in 150–400 µm clear films. A masterbatch pre-disperses Sb2O3 in a matched carrier, keeping haze < 2–3% at target wall.
- Dust-free handling — no airborne fine powder on thermoforming or extrusion lines, safer and cleaner dosing by loss-in-weight feeder.
- Lot consistency — Sb2O3 content fixed per batch, giving repeatable flame-retardant response and optical appearance from run to run.
2. Carrier & formulation matching
- Carrier — use a rigid-PVC / K-value 55–60 compatible carrier, or an EVA/CPE polarity-matched carrier; do not use a low-K carrier that plasticizes the compound.
- Halogen–Sb synergy — with chlorinated paraffin (CP-52/70) target Cl:Sb ≈ 3:1 molar; when co-using brominated FRs recalculate on effective halogen, not compound weight.
- Thermal stabilizer balance — pair with Ca-Zn stabilizer; Sb2O3 can raise the degradation onset, so re-check the stability window and plate-out risk on the die.
3. Processing & QC checkpoints
- Pre-dry — dry masterbatch 2–4 h at 80 °C if stored above 60% RH to prevent moisture streaking.
- Melt temperature — keep melt ≤ 190 °C; watch die/calibration plate-out and screen-pack pressure rise as a dispersion proxy.
- Optical checks — measure haze and transmittance on trial plaques before batch commitment; look for white specks under transmitted light.
- Reaction-to-fire — run EN 13501-1 / UL 94 at the target final wall thickness, not on thick plaques.
4. Supplier qualification (CoA per lot)
- Purity ≥ 99.5%
- Moisture < 0.3%
- D50 0.8–1.5 µm fine grade (critical for optical clarity)
- Pb < 50 ppm, Fe < 100 ppm, whiteness consistency ≥ 96
- Retain 200 g per-lot sample for 12 months for traceability and dispute resolution.